Thermal Conductivity and Debye Temperature

Li
344
0.85
Be
1440
2.00
Debye temperature and thermal conductivity
Low temperature limit of Debye temperature in Kelvin
Thermal conductivity at 300K, in W/cmK
B
...
0.27
C
2230
1.29
N
...
...
O
...
...
F
...
...
Ne
75
...
Na
158
1.41
Mg
400
1.56
...
Al
428
2.37
Si
645
1.48
P
...
...
S
...
...
Cl
...
...
Ar
92
...
K
91
1.02
Ca
230
...
Sc
360
0.16
Ti
420
0.22
V
380
0.31
Cr
630
0.94
Mn
410
0.08
Fe
470
0.80
Co
445
1.00
Ni
450
0.91
Cu
343
4.01
Zn
327
1.16
Ga
320
0.41
Ge
374
0.6
As
282
0.50
Se
90
0.02
Br
...
...
Kr
72
...
Rb
56
0.58
Sr
147
...
Y
280
0.17
Zr
291
0.23
Nb
275
0.54
Mo
450
1.38
Tc
...
0.51
Ru
600
1.17
Rh
480
1.50
Pd
274
0.72
Ag
225
4.29
Cd
209
0.97
In
108
0.82
Sn
200
0.67
Sb
211
0.24
Te
153
0.02
I
...
...
Xe
64
...
Cs
38
0.36
Ba
110
...
La
142
0.14
Hf
252
0.23
Ta
240
0.58
W
400
1.74
Re
430
0.48
Os
500
0.88
Ir
420
1.47
Pt
240
0.72
Au
165
3.17
Hg
71.9
...
Tl
78.5
0.46
Pb
105
0.35
Bi
119
0.08
Po
...
...
At
...
...
Rn
64
...
Fr
...
...
Ra
...
...
Ac
...
...
...
...
Ce
...
0.11
Pr
...
0.13
Nd
...
0.16
Pm
...
...
Sm
...
0.13
Eu
...
...
Gd
200
0.11
Tb
...
0.11
Dy
210
0.11
Ho
...
0.16
Er
...
0.14
Tm
...
0.17
Yb
120
0.35
Lu
210
0.16
...
...
Th
163
0.54
Pa
...
...
U
207
0.28
Np
...
0.06
Pu
...
0.07
Am
...
...
Cm
...
...
Bk
...
...
Cf
...
...
Es
...
...
Fm
...
...
Md
...
...
No
...
...
Lr
...
...
...
Data from Kittel, Introduction to Solid State Physic, 7th Ed.